Molybdenum Tubes For Sapphire Crystal Growth Furnaces

Molybdenum Tubes For Sapphire Crystal Growth Furnaces
Details:
Material: High-purity molybdenum
Product Name: Sapphire furnace Mo tube
MOQ: Small trial orders accepted
Chemical Composition: Mo ≥99.95%
Standard: Custom per drawing
Size Tolerance: Strict wall control
Dimensional Accuracy: Full-length checked
Surface roughness: Clean oil-free annealed
Send Inquiry
Description
Send Inquiry

Products Description

Sapphire is single crystal alpha-Al2O3. It has a melting point of approximately 2050 C, and during crystal growth the melting point will be around 2100 C. There are very few materials suitable for continuous operation in such a high temperature environment. The two main options are tungsten and molybdenum. The molybdenum tube itself will not carry the molten material. The tube will support the crucible, provide accurate temperature measurement, provide current to the hot zone, and provide gas and vision routing. The tube will have a hollow section. This is not to save material but to reduce the overall weight. It will also aid with wiring, venting of gases and allow a thermocouple to go through the centre. The four areas below will explain where the tube will sit, what you can control, what type of furnace it will go in, and what you should consider when ordering.

 

4 areas the tube will be in the hot zone:

Crucible post

During Kyropoulos crystal growth, the crucible is mounted onto a vertical post. The crystal is grown from within the crucible. The entire weight and thermal load of the furnace is transferred through this tube. It needs to be robust enough to withstand the high temperatures without collapsing, concentric to the heater, and return to original height on each time the furnace is rebuilt. If the wall is too thin the tube will visibly sag during the latter stages of operation. the crucible base then loses consistent contact with the heat exchange surface or seat. There will also be a drift in the thermal field.

Thermocouple sheath

Most furnaces use tungsten-rhenium thermocouples due to the high melt temps (>2000C). The sheath will protect the wires from the melt and atmosphere. The wall thickness will need to be a compromise between fast response time and longevity. Thin walled tubes will give a fast response but will have poor erosion and distortion resistance. Thick walled tubes will be long lasting but will suffer from a noticeable delay in thermal response. The end weld must be leak tight. Any pinhole will cause the wires to drift after a few runs.

Heater lead and connection pipe

The current from the heater is passed into the water cooled electrode or copper busbar. There may be some concerns about contact resistance, seal, and thermal expansion. Once the threads/flanges have seized due to the heat, the part would need to be replaced and would require the whole hot zone to be worked on.

 

Draft tube, vision tube and gas inlet

Internal heat shield tubes, vision tubes and Argon/Hydrogen mix pipes will all be thin walled long tubes. These will have no load but will be sensitive to roundness, straightness and cleanliness. If the roundness of the tube is out then the thermal shielding will be affected. The interface temperature will drift.

Molybdenum Tubes in Sapphire Growth Furnaces Crucible post

 

Purity

The purity of the material will be grade Mo1 (99.95%+). We will provide material certification for the batch. Sapphire is highly sensitive to transition metals. Migration of Iron, Nickel, and Chromium at 2000C will show directly with colouration of the crystal or absorption peaks. Density and grain structure are harder to notice but will affect the lifespan of the material. If the billet is coarse grained or has any porosity left in then the grains will continue to grow during crystal growth reducing creep resistance. There will be visible sagging and ovality after a few runs.

 
 
 
 

Wall thickness and concentricity

 

 

 

Wall thickness and concentricity should be shown on the drawing. The wall is the only area of creep compensation. Usually the thin section will be in the direction of the highest heat from the heater if the tube is eccentric.

 
 
 

Straightness and roundness

 

 

The straightness and roundness of the tube will be measured and documented throughout the whole length and in sections. The end shape should be decided (Flange, Thread, Taper, Weld Plug), and the disassembly of the part after use. This is because recrystallized molybdenum will crack easiest at threads and weld heat affected zones.

product parameters

Characteristic

What we control Why it matters in a sapphire hot zone
Grade and purity Mo1, ≥99.95% Mo, certificate per batch Fe, Ni, Cr and alkali residuals volatilise or migrate into the melt and show up as colour centres or inclusions
Density and grain Near-theoretical density, fine uniform grain, no connected porosity Porosity and coarse grain accelerate grain growth, sag and crack initiation at 2,000 °C
Wall thickness Minimum wall at the hot zone, measured concentricity The wall is the only creep allowance; eccentric wall puts the thin side in the hottest position
Straightness and ovality Measured over the full length, per section A tube that is oval will not seal, and an oval shield sleeve shifts the thermal gradient
End form and finish Flange, thread, taper or welded plug; annealed, cleaned, dry-packed Joints and threads are where recrystallised parts crack during disassembly

Molybdenum Tubes in Sapphire Growth Furnaces Heater lead and connection pipe

Decide before ordering

 

Furnace type and crystal growth method. This will dictate how the part will be fitted in the hot zone. Melt temp and power distribution. The heater will have zones and the power per zone. This will determine the thermal gradient the wall will experience. Interface dimensions. Flanges, threads and locating steps should be clearly marked. Don't want to fit from an outline drawing with each party having their own datum. Atmosphere. How much vacuum, Argon purity, Hydrogen level and dew point. Molybdenum will oxidise in the presence of Oxygen or high levels of moisture. This is completely different to a glass furnace. Clamping and thermal expansion. How much radial clearance and point contact allowed. This should be shown on the drawing. Acceptance criteria. Measured dimensions, wall thickness, visual, penetrant/radiography and metallography if required. Material certification for the batch.

 

 

Electrode stock will follow YS/T 1312-2019. Molybdenum rod will follow ASTM B387 / GB/T 17792. Plate and Disc will follow ASTM B386 / GB/T 3876. Pipe fittings generally won't have a specific product standard so the drawing, minimum wall thickness, inspection and acceptance criteria will be your whole quality. It is much more effective to put this in the technical agreement.
Please send us the furnace type, hot zone parameters and interface drawings. We will respond with material suggestions, wall thickness suggestions and lead time based on the drawing.

 

 

NAME

           Ava 

wechat

           18291778622

LinkedIn

           ava20250912@gmail.com

WhatsApp

          +86 182 9177 8622

E-mail

           Zr-Hf@titanmsgp.com

Molybdenum Tubes in Sapphire Growth Furnaces Thermocouple sheath

 

 

Hot Tags: molybdenum tubes for sapphire crystal growth furnaces, China molybdenum tubes for sapphire crystal growth furnaces manufacturers, suppliers, factory, Molybdenum Alloy Pipe, molybdenum tube

Send Inquiry